Superalloy Investment Castings Market by Alloy, Application, Component, Process, Distribution Channel - Global Forecast to 2030

  • PDF Icon

    Report

  • 194 Pages
  • May 2025
  • Region: Global
  • 360iResearch™
  • ID: 6085402
UP TO OFF until Dec 31st 2025
1h Free Analyst Time
1h Free Analyst Time

Speak directly to the analyst to clarify any post sales queries you may have.

The superalloy investment casting market is undergoing significant change as emerging technologies, regulatory shifts, and evolving industrial needs reshape the value chain. Global organizations that rely on critical components for aerospace propulsion, power generation, and advanced industrial applications are recalibrating sourcing, supply chain, and manufacturing strategies to maintain resilience and performance leadership in an intensifying competitive landscape.

Market Snapshot: Superalloy Investment Casting Market

The global superalloy investment casting market is a vital segment within the advanced materials sector, driven by demand for high-performance components in industries that require exceptional strength, thermal stability, and corrosion resistance under extreme operating conditions. The sector is anchored by applications in aerospace, power generation, oil & gas, automotive, medical, and petrochemical industries. Stakeholders are pursuing tighter tolerances, complex geometries, and superior surface finishes, while navigating an ecosystem shaped by innovation, regulatory changes, and global trade dynamics. The market size and growth rate reflect robust long-term prospects amidst ongoing modernization and sustainability initiatives.

Scope & Segmentation of the Superalloy Investment Casting Market

  • Alloy Types: Cobalt, Iron, Nickel
  • Applications: Aerospace (Civil, Military), Automotive, Medical, Petrochemical, Oil & Gas (Downstream, Midstream, Upstream), Power Generation (Gas Turbines, Steam Turbines)
  • Components: Structural Components, Turbine Blades, Turbine Discs, Vanes
  • Process Technologies: Ceramic Shell, Lost Wax, Vacuum Investment
  • Distribution Channels: Aftermarket (Authorized Service Centers, Independent MRO), OEM (Direct Sales, Distributor Sales)
  • Regional Coverage: Americas (United States—California, Texas, New York, Florida, Illinois, Pennsylvania, Ohio; Canada; Mexico; Brazil; Argentina), Europe, Middle East & Africa (United Kingdom, Germany, France, Russia, Italy, Spain, United Arab Emirates, Saudi Arabia, South Africa, Denmark, Netherlands, Qatar, Finland, Sweden, Nigeria, Egypt, Turkey, Israel, Norway, Poland, Switzerland), Asia-Pacific (China, India, Japan, Australia, South Korea, Indonesia, Thailand, Philippines, Malaysia, Singapore, Vietnam, Taiwan)
  • Industry Leaders Profiled: Precision Castparts Corp., Howmet Aerospace Inc., Aubert & Duval SAS, voestalpine AG, Hitachi Metals, Ltd., CMK Corporation, Alcoa Corporation, GKN Aerospace Services Limited, Sandvik AB, Allegheny Technologies Incorporated

Key Takeaways for Senior Decision-Makers

  • Integration of advanced digital design and simulation tools is accelerating product development, enabling optimization of alloy compositions and geometries for more reliable and efficient components.
  • Sustainability requirements are reshaping production practices, prompting adoption of low-emission melting techniques and leaner processes to meet carbon reduction targets.
  • Supply chain diversification and regionalization are now strategic imperatives, as geopolitical and trade uncertainties impact raw material sourcing and market access.
  • Detailed market segmentation enables precise targeting of high-growth segments, including aerospace and power generation, where superalloy investment casting delivers performance and longevity gains.
  • Industry consolidation and technological innovation are fostering collaboration, deeper integration, and the emergence of specialized foundries dedicated to critical, high-value applications.

Tariff Impact: 2025 U.S. Trade Policy Considerations

Upcoming United States tariffs in 2025 are poised to alter cost structures, particularly for imported alloying elements and finished components. These trade measures are prompting strategic shifts, from supplier reassessment to the establishment of local production partnerships and joint ventures within tariff-exempt regions. End users are mitigating risk by leveraging long-term contracts and supplier audits to manage fluctuating costs and maintain continuity of supply.

Methodology & Data Sources

Research insights are grounded in a combination of primary interviews with senior executives, technical specialists, and procurement managers, alongside secondary analysis from industry publications, regulatory filings, and corporate disclosures. Data triangulation ensures credibility and a multi-dimensional perspective across all key market segments, regions, and application areas.

Why This Report Matters

  • Pinpoints critical trends and disruptive forces enabling leaders to refine growth, investment, and risk mitigation strategies.
  • Provides granular segmentation and regional analysis to identify new opportunities in evolving and emerging markets.
  • Equips stakeholders with actionable intelligence for navigating complexity from innovation, regulations, and shifting supply chains.

Conclusion

The superalloy investment casting market is navigating transformation through digitalization, sustainability priorities, and regulatory dynamics. Segment-focused strategies and regional insights are vital for organizations seeking resilience and competitive advantage in a rapidly evolving global environment.



This product will be delivered within 1-3 business days.

Table of Contents

1. Preface
1.1. Objectives of the Study
1.2. Market Segmentation & Coverage
1.3. Years Considered for the Study
1.4. Currency & Pricing
1.5. Language
1.6. Stakeholders
2. Research Methodology
2.1. Define: Research Objective
2.2. Determine: Research Design
2.3. Prepare: Research Instrument
2.4. Collect: Data Source
2.5. Analyze: Data Interpretation
2.6. Formulate: Data Verification
2.7. Publish: Research Report
2.8. Repeat: Report Update
3. Executive Summary
4. Market Overview
4.1. Introduction
4.2. Market Sizing & Forecasting
5. Market Dynamics
6. Market Insights
6.1. Porter’s Five Forces Analysis
6.2. PESTLE Analysis
7. Cumulative Impact of United States Tariffs 2025
8. Superalloy Investment Castings Market, by Alloy
8.1. Introduction
8.2. Cobalt
8.3. Iron
8.4. Nickel
9. Superalloy Investment Castings Market, by Application
9.1. Introduction
9.2. Aerospace
9.2.1. Civil Aerospace
9.2.2. Military Aerospace
9.3. Industrial
9.3.1. Automotive
9.3.2. Medical
9.3.3. Petrochemical
9.4. Oil & Gas
9.4.1. Downstream
9.4.2. Midstream
9.4.3. Upstream
9.5. Power Generation
9.5.1. Gas Turbines
9.5.2. Steam Turbines
10. Superalloy Investment Castings Market, by Component
10.1. Introduction
10.2. Structural Components
10.3. Turbine Blades
10.4. Turbine Discs
10.5. Vanes
11. Superalloy Investment Castings Market, by Process
11.1. Introduction
11.2. Ceramic Shell
11.3. Lost Wax
11.4. Vacuum Investment
12. Superalloy Investment Castings Market, by Distribution Channel
12.1. Introduction
12.2. Aftermarket
12.2.1. Authorized Service Centers
12.2.2. Independent MRO
12.3. OEM
12.3.1. Direct Sales
12.3.2. Distributor Sales
13. Americas Superalloy Investment Castings Market
13.1. Introduction
13.2. United States
13.3. Canada
13.4. Mexico
13.5. Brazil
13.6. Argentina
14. Europe, Middle East & Africa Superalloy Investment Castings Market
14.1. Introduction
14.2. United Kingdom
14.3. Germany
14.4. France
14.5. Russia
14.6. Italy
14.7. Spain
14.8. United Arab Emirates
14.9. Saudi Arabia
14.10. South Africa
14.11. Denmark
14.12. Netherlands
14.13. Qatar
14.14. Finland
14.15. Sweden
14.16. Nigeria
14.17. Egypt
14.18. Turkey
14.19. Israel
14.20. Norway
14.21. Poland
14.22. Switzerland
15. Asia-Pacific Superalloy Investment Castings Market
15.1. Introduction
15.2. China
15.3. India
15.4. Japan
15.5. Australia
15.6. South Korea
15.7. Indonesia
15.8. Thailand
15.9. Philippines
15.10. Malaysia
15.11. Singapore
15.12. Vietnam
15.13. Taiwan
16. Competitive Landscape
16.1. Market Share Analysis, 2024
16.2. FPNV Positioning Matrix, 2024
16.3. Competitive Analysis
16.3.1. Precision Castparts Corp.
16.3.2. Howmet Aerospace Inc.
16.3.3. Aubert & Duval SAS
16.3.4. voestalpine AG
16.3.5. Hitachi Metals, Ltd.
16.3.6. CMK Corporation
16.3.7. Alcoa Corporation
16.3.8. GKN Aerospace Services Limited
16.3.9. Sandvik AB
16.3.10. Allegheny Technologies Incorporated
17. ResearchAI
18. ResearchStatistics
19. ResearchContacts
20. ResearchArticles
21. Appendix
List of Figures
FIGURE 1. SUPERALLOY INVESTMENT CASTINGS MARKET MULTI-CURRENCY
FIGURE 2. SUPERALLOY INVESTMENT CASTINGS MARKET MULTI-LANGUAGE
FIGURE 3. SUPERALLOY INVESTMENT CASTINGS MARKET RESEARCH PROCESS
FIGURE 4. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, 2018-2030 (USD MILLION)
FIGURE 5. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY REGION, 2024 VS 2025 VS 2030 (USD MILLION)
FIGURE 6. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COUNTRY, 2024 VS 2025 VS 2030 (USD MILLION)
FIGURE 7. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2024 VS 2030 (%)
FIGURE 8. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2024 VS 2025 VS 2030 (USD MILLION)
FIGURE 9. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2024 VS 2030 (%)
FIGURE 10. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2024 VS 2025 VS 2030 (USD MILLION)
FIGURE 11. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2024 VS 2030 (%)
FIGURE 12. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2024 VS 2025 VS 2030 (USD MILLION)
FIGURE 13. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2024 VS 2030 (%)
FIGURE 14. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2024 VS 2025 VS 2030 (USD MILLION)
FIGURE 15. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2024 VS 2030 (%)
FIGURE 16. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2024 VS 2025 VS 2030 (USD MILLION)
FIGURE 17. AMERICAS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COUNTRY, 2024 VS 2030 (%)
FIGURE 18. AMERICAS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COUNTRY, 2024 VS 2025 VS 2030 (USD MILLION)
FIGURE 19. UNITED STATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY STATE, 2024 VS 2030 (%)
FIGURE 20. UNITED STATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY STATE, 2024 VS 2025 VS 2030 (USD MILLION)
FIGURE 21. EUROPE, MIDDLE EAST & AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COUNTRY, 2024 VS 2030 (%)
FIGURE 22. EUROPE, MIDDLE EAST & AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COUNTRY, 2024 VS 2025 VS 2030 (USD MILLION)
FIGURE 23. ASIA-PACIFIC SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COUNTRY, 2024 VS 2030 (%)
FIGURE 24. ASIA-PACIFIC SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COUNTRY, 2024 VS 2025 VS 2030 (USD MILLION)
FIGURE 25. SUPERALLOY INVESTMENT CASTINGS MARKET SHARE, BY KEY PLAYER, 2024
FIGURE 26. SUPERALLOY INVESTMENT CASTINGS MARKET, FPNV POSITIONING MATRIX, 2024
List of Tables
TABLE 1. SUPERALLOY INVESTMENT CASTINGS MARKET SEGMENTATION & COVERAGE
TABLE 2. UNITED STATES DOLLAR EXCHANGE RATE, 2018-2024
TABLE 3. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, 2018-2030 (USD MILLION)
TABLE 4. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY REGION, 2018-2030 (USD MILLION)
TABLE 5. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COUNTRY, 2018-2030 (USD MILLION)
TABLE 6. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 7. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COBALT, BY REGION, 2018-2030 (USD MILLION)
TABLE 8. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY IRON, BY REGION, 2018-2030 (USD MILLION)
TABLE 9. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY NICKEL, BY REGION, 2018-2030 (USD MILLION)
TABLE 10. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 11. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, BY REGION, 2018-2030 (USD MILLION)
TABLE 12. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY CIVIL AEROSPACE, BY REGION, 2018-2030 (USD MILLION)
TABLE 13. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY MILITARY AEROSPACE, BY REGION, 2018-2030 (USD MILLION)
TABLE 14. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 15. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, BY REGION, 2018-2030 (USD MILLION)
TABLE 16. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AUTOMOTIVE, BY REGION, 2018-2030 (USD MILLION)
TABLE 17. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY MEDICAL, BY REGION, 2018-2030 (USD MILLION)
TABLE 18. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PETROCHEMICAL, BY REGION, 2018-2030 (USD MILLION)
TABLE 19. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 20. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, BY REGION, 2018-2030 (USD MILLION)
TABLE 21. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DOWNSTREAM, BY REGION, 2018-2030 (USD MILLION)
TABLE 22. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY MIDSTREAM, BY REGION, 2018-2030 (USD MILLION)
TABLE 23. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY UPSTREAM, BY REGION, 2018-2030 (USD MILLION)
TABLE 24. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 25. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, BY REGION, 2018-2030 (USD MILLION)
TABLE 26. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY GAS TURBINES, BY REGION, 2018-2030 (USD MILLION)
TABLE 27. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY STEAM TURBINES, BY REGION, 2018-2030 (USD MILLION)
TABLE 28. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 29. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 30. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY STRUCTURAL COMPONENTS, BY REGION, 2018-2030 (USD MILLION)
TABLE 31. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY TURBINE BLADES, BY REGION, 2018-2030 (USD MILLION)
TABLE 32. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY TURBINE DISCS, BY REGION, 2018-2030 (USD MILLION)
TABLE 33. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY VANES, BY REGION, 2018-2030 (USD MILLION)
TABLE 34. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 35. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY CERAMIC SHELL, BY REGION, 2018-2030 (USD MILLION)
TABLE 36. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY LOST WAX, BY REGION, 2018-2030 (USD MILLION)
TABLE 37. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY VACUUM INVESTMENT, BY REGION, 2018-2030 (USD MILLION)
TABLE 38. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 39. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, BY REGION, 2018-2030 (USD MILLION)
TABLE 40. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AUTHORIZED SERVICE CENTERS, BY REGION, 2018-2030 (USD MILLION)
TABLE 41. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDEPENDENT MRO, BY REGION, 2018-2030 (USD MILLION)
TABLE 42. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 43. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, BY REGION, 2018-2030 (USD MILLION)
TABLE 44. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DIRECT SALES, BY REGION, 2018-2030 (USD MILLION)
TABLE 45. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTOR SALES, BY REGION, 2018-2030 (USD MILLION)
TABLE 46. GLOBAL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 47. AMERICAS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 48. AMERICAS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 49. AMERICAS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 50. AMERICAS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 51. AMERICAS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 52. AMERICAS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 53. AMERICAS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 54. AMERICAS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 55. AMERICAS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 56. AMERICAS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 57. AMERICAS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 58. AMERICAS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COUNTRY, 2018-2030 (USD MILLION)
TABLE 59. UNITED STATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 60. UNITED STATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 61. UNITED STATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 62. UNITED STATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 63. UNITED STATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 64. UNITED STATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 65. UNITED STATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 66. UNITED STATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 67. UNITED STATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 68. UNITED STATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 69. UNITED STATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 70. UNITED STATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY STATE, 2018-2030 (USD MILLION)
TABLE 71. CANADA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 72. CANADA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 73. CANADA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 74. CANADA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 75. CANADA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 76. CANADA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 77. CANADA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 78. CANADA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 79. CANADA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 80. CANADA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 81. CANADA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 82. MEXICO SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 83. MEXICO SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 84. MEXICO SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 85. MEXICO SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 86. MEXICO SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 87. MEXICO SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 88. MEXICO SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 89. MEXICO SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 90. MEXICO SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 91. MEXICO SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 92. MEXICO SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 93. BRAZIL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 94. BRAZIL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 95. BRAZIL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 96. BRAZIL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 97. BRAZIL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 98. BRAZIL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 99. BRAZIL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 100. BRAZIL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 101. BRAZIL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 102. BRAZIL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 103. BRAZIL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 104. ARGENTINA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 105. ARGENTINA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 106. ARGENTINA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 107. ARGENTINA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 108. ARGENTINA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 109. ARGENTINA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 110. ARGENTINA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 111. ARGENTINA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 112. ARGENTINA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 113. ARGENTINA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 114. ARGENTINA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 115. EUROPE, MIDDLE EAST & AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 116. EUROPE, MIDDLE EAST & AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 117. EUROPE, MIDDLE EAST & AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 118. EUROPE, MIDDLE EAST & AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 119. EUROPE, MIDDLE EAST & AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 120. EUROPE, MIDDLE EAST & AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 121. EUROPE, MIDDLE EAST & AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 122. EUROPE, MIDDLE EAST & AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 123. EUROPE, MIDDLE EAST & AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 124. EUROPE, MIDDLE EAST & AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 125. EUROPE, MIDDLE EAST & AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 126. EUROPE, MIDDLE EAST & AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COUNTRY, 2018-2030 (USD MILLION)
TABLE 127. UNITED KINGDOM SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 128. UNITED KINGDOM SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 129. UNITED KINGDOM SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 130. UNITED KINGDOM SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 131. UNITED KINGDOM SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 132. UNITED KINGDOM SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 133. UNITED KINGDOM SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 134. UNITED KINGDOM SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 135. UNITED KINGDOM SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 136. UNITED KINGDOM SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 137. UNITED KINGDOM SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 138. GERMANY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 139. GERMANY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 140. GERMANY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 141. GERMANY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 142. GERMANY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 143. GERMANY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 144. GERMANY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 145. GERMANY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 146. GERMANY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 147. GERMANY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 148. GERMANY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 149. FRANCE SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 150. FRANCE SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 151. FRANCE SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 152. FRANCE SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 153. FRANCE SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 154. FRANCE SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 155. FRANCE SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 156. FRANCE SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 157. FRANCE SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 158. FRANCE SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 159. FRANCE SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 160. RUSSIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 161. RUSSIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 162. RUSSIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 163. RUSSIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 164. RUSSIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 165. RUSSIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 166. RUSSIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 167. RUSSIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 168. RUSSIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 169. RUSSIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 170. RUSSIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 171. ITALY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 172. ITALY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 173. ITALY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 174. ITALY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 175. ITALY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 176. ITALY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 177. ITALY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 178. ITALY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 179. ITALY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 180. ITALY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 181. ITALY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 182. SPAIN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 183. SPAIN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 184. SPAIN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 185. SPAIN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 186. SPAIN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 187. SPAIN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 188. SPAIN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 189. SPAIN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 190. SPAIN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 191. SPAIN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 192. SPAIN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 193. UNITED ARAB EMIRATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 194. UNITED ARAB EMIRATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 195. UNITED ARAB EMIRATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 196. UNITED ARAB EMIRATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 197. UNITED ARAB EMIRATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 198. UNITED ARAB EMIRATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 199. UNITED ARAB EMIRATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 200. UNITED ARAB EMIRATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 201. UNITED ARAB EMIRATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 202. UNITED ARAB EMIRATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 203. UNITED ARAB EMIRATES SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 204. SAUDI ARABIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 205. SAUDI ARABIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 206. SAUDI ARABIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 207. SAUDI ARABIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 208. SAUDI ARABIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 209. SAUDI ARABIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 210. SAUDI ARABIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 211. SAUDI ARABIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 212. SAUDI ARABIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 213. SAUDI ARABIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 214. SAUDI ARABIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 215. SOUTH AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 216. SOUTH AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 217. SOUTH AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 218. SOUTH AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 219. SOUTH AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 220. SOUTH AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 221. SOUTH AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 222. SOUTH AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 223. SOUTH AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 224. SOUTH AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 225. SOUTH AFRICA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 226. DENMARK SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 227. DENMARK SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 228. DENMARK SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 229. DENMARK SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 230. DENMARK SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 231. DENMARK SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 232. DENMARK SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 233. DENMARK SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 234. DENMARK SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 235. DENMARK SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 236. DENMARK SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 237. NETHERLANDS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 238. NETHERLANDS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 239. NETHERLANDS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 240. NETHERLANDS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 241. NETHERLANDS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 242. NETHERLANDS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 243. NETHERLANDS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 244. NETHERLANDS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 245. NETHERLANDS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 246. NETHERLANDS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 247. NETHERLANDS SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 248. QATAR SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 249. QATAR SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 250. QATAR SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 251. QATAR SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 252. QATAR SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 253. QATAR SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 254. QATAR SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 255. QATAR SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 256. QATAR SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 257. QATAR SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 258. QATAR SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 259. FINLAND SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 260. FINLAND SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 261. FINLAND SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 262. FINLAND SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 263. FINLAND SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 264. FINLAND SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 265. FINLAND SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 266. FINLAND SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 267. FINLAND SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 268. FINLAND SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 269. FINLAND SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 270. SWEDEN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 271. SWEDEN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 272. SWEDEN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 273. SWEDEN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 274. SWEDEN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 275. SWEDEN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 276. SWEDEN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 277. SWEDEN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 278. SWEDEN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 279. SWEDEN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 280. SWEDEN SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 281. NIGERIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 282. NIGERIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 283. NIGERIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 284. NIGERIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 285. NIGERIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 286. NIGERIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 287. NIGERIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 288. NIGERIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 289. NIGERIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 290. NIGERIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 291. NIGERIA SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 292. EGYPT SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 293. EGYPT SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 294. EGYPT SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 295. EGYPT SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 296. EGYPT SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 297. EGYPT SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 298. EGYPT SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 299. EGYPT SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 300. EGYPT SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 301. EGYPT SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 302. EGYPT SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 303. TURKEY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 304. TURKEY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY APPLICATION, 2018-2030 (USD MILLION)
TABLE 305. TURKEY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AEROSPACE, 2018-2030 (USD MILLION)
TABLE 306. TURKEY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY INDUSTRIAL, 2018-2030 (USD MILLION)
TABLE 307. TURKEY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OIL & GAS, 2018-2030 (USD MILLION)
TABLE 308. TURKEY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY POWER GENERATION, 2018-2030 (USD MILLION)
TABLE 309. TURKEY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY COMPONENT, 2018-2030 (USD MILLION)
TABLE 310. TURKEY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY PROCESS, 2018-2030 (USD MILLION)
TABLE 311. TURKEY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY DISTRIBUTION CHANNEL, 2018-2030 (USD MILLION)
TABLE 312. TURKEY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY AFTERMARKET, 2018-2030 (USD MILLION)
TABLE 313. TURKEY SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY OEM, 2018-2030 (USD MILLION)
TABLE 314. ISRAEL SUPERALLOY INVESTMENT CASTINGS MARKET SIZE, BY ALLOY, 2018-2030 (USD MILLION)
TABLE 315. ISRAEL SUPERALLOY INVESTMENT CASTINGS MARKE

Samples

Loading
LOADING...

Companies Mentioned

The companies profiled in this Superalloy Investment Castings market report include:
  • Precision Castparts Corp.
  • Howmet Aerospace Inc.
  • Aubert & Duval SAS
  • voestalpine AG
  • Hitachi Metals, Ltd.
  • CMK Corporation
  • Alcoa Corporation
  • GKN Aerospace Services Limited
  • Sandvik AB
  • Allegheny Technologies Incorporated